Wear & Tear of a Spinning Front Line Rubber Cot
|
|
By
:
B. Sujai
|
|
|
|
|
Wear & Tear of a Spinning Front
Line Rubber Cot and Factors Affecting it in Terms of Usage, Abrasion Resistance
of That Rubber Compound, Traverse Length, Traverse Rate, Shore a Hardness, Top
Arm Loading, Fibre Volume Handled and Frictional Properties of the Processed
Material
Abstract
In general yarn quality is influenced by:
- Quality of raw material
- Opening & cleaning operations at Blow room &
Carding
- Speeds & Settings kept at various stages of yarn
production and its functions.
- Process control techniques and parameters kept at
spinning
- Humidification, (temperature and humidity)
- Labour force training and their skills.
- Maintenance of production equipment and vital
components.
Drafting components have a significant influence on yarn
quality and production costs in ring spinning. Especially spinning top roller
covers i.e., cots and drafting aprons. These are the main components of the drafting
mechanism and certainly it has more influence on the quality of the yarn
produced. Apart from above mentioned factors that decide ultimate quality of
yarn there are other factors which has a major influence on yarn quality like shore
a hardness of rubber cot used, wear out rate of the cot in traverse area, abrasion
resistance of the rubber compound and other parameters kept at spinning.
Read
Full Article